PA 6/6 Injection Molding – 20%-40% Mineral Reinforced

Processing Considerations for PA 6/6 Injection Molding – 20%-40% Mineral Reinforced

Recommended Processing Considerations: PA 6/6 Injection Molding - 20%-40% Mineral Reinforced

Drying Temperature
180°F (82°C)
Drying Time2-4 hrs. max.
Maximum Moisture0.002%
Rear
480-540°F  (249-282°C)
Middle
520-560°F (271-293°C)
Front
520-560°F (271-293°C)
Nozzel
520-560°F (271-293°C)
Melt Temperature
520-540°F (271-282)°C)
Mold Temperature
80-160°F (27-71°C)
Back Pressure
50 to 100 psi