Very High Impact Resistance

Processing Considerations for Very High Impact Resistance

Recommended Processing Considerations: Very High Impact Resistance

Drying Temperature
180°F (82°C)
Drying Time2-4 hrs. max
Maximum Moisture0.20%
Rear
460-520°F  (238-271°C)
Middle
480-520°F (249-271°C)
Front
480-520°F (249-271°C)
Nozzel
480-560°F (249-293°C)
Melt Temperature
480-560°F (249-293)°C)
Mold Temperature
80-160°F (27-71°C)
Back Pressure
50 to 100 psi