| Pressure | psi |
|---|---|
| Injection | 4 – 12,000 |
| Hold | 3 – 9,000 |
| Back | 0 – 50 |
Maximum Moisture: 0.2%
Mold Temperature:
150-250 °F, highly filled grades require >175 °F to obtain the best overall surface appearance
Residence Time:
Should not exceed 6 minutes, less with higher melt temps.
Shot Size:
Should be between 25-75% of barrel capacity.
Fill Rate:
Fast fill rates are suggested for best surface appearance.
Regrind Level:
Typically no more than 25% is recommended, with higher levels possible for unfilled grades depending on the end use requirements. Make certain regrind is properly dried to virgin moisture levels.
Drying Temp.
Nylene 6/12 – 150-180 °F for 2-4 hours
Nylene 6250L is a low viscosity nylon 6/12 molding resin. This material us used in applications requiring good electrical insulation properties. When molding, Nylene 6250L has high flow characteristics at minimum temperatures.